Variation of liquation cracking susceptibility for overaged 247LC superalloy repair weld heataffected zone
장시간 열간노출에 따른 247LC 초내열합금 보수용접 열영향부의 액화균열민감도 변화
Hye-Eun Jeong, Seong-Moon Seo, Eun-Joon Chun
정혜은, 서성문, 천은준
Korean J. Met. Mater. 2023;61(2):69-75.   Published online 2023 Jan 27
DOI: https://doi.org/10.3365/KJMM.2023.61.2.69

Abstract
In this study, the liquation cracking temperature range (LCTR) of over-aged 247LC superalloy repair welds was quantitatively evaluated using spot-Varestraint testing, especially for application in the repair weld heat-affected zone (HAZ). The metallurgical mechanism of the evaluated liquation cracking susceptibility and variation of the LCTRs of the over-aged 247LC superalloys..... More

                   Web of Science 1  Crossref 2
Evaluation of Liquation Cracking Susceptibility of CM247LC Superalloy Repair Welds via Pre-Weld Varestraint Test
Pre-weld Varestraint 시험을 이용한 CM247LC 초내열합금 보수용접부 액화균열 민감도 평가
Ye-Seon Jeong, Jingon Jeong, Se-Yun Kim, Sung-Hwan Bae, Uijong Lee, Hyungsoo Lee, Seong-Moon Seo, Eun-Joon Chun
정예선, 정진곤, 김세윤, 배성환, 이의종, 이형수, 서성문, 천은준
Korean J. Met. Mater. 2022;60(4):272-281.   Published online 2022 Mar 28
DOI: https://doi.org/10.3365/KJMM.2022.60.4.272

Abstract
In this study, the liquation cracking susceptibility in the heat-affected zone of CM247LC superalloy gas turbine blades during repair welding was quantitatively evaluated using a newly developed pre-weld Varestraint test method. The repair welding geometry was replicated through Varestraint tests for the pre-weld bead. The liquation cracking susceptibility, that is,..... More

                   Web of Science 3  Crossref 5
Effect of ERNiFeCr-2 Filler Metal on Solidification Cracking Susceptibility of CM247LC Superalloy Welds
ERNiFeCr-2 용가재 적용에 따른 CM247LC 초내열합금 용접부 응고균열 민감도 변화 거동
Kyeong-Min Kim, Hye-Eun Jeong, Ye-Seon Jeong, Uijong Lee, Hyungsoo Lee, Seong-Moon Seo, Eun-Joon Chun
김경민, 정혜은, 정예선, 이의종, 이형수, 서성문, 천은준
Korean J. Met. Mater. 2021;59(10):698-708.   Published online 2021 Sep 6
DOI: https://doi.org/10.3365/KJMM.2021.59.10.698

Abstract
The metallurgical aspects of weld solidification cracking in Ni-based superalloys (with Ti+Al > 5 mass%) have not been widely investigated thus far. Herein, the solidification cracking susceptibility of the CM247LC superalloy and its welds with ERNiFeCr-2 filler wire was quantitatively evaluated using a novel modified Varestraint testing method, for the..... More

                   Crossref 2
Evaluation and Control of Liquation Cracking Susceptibility for CM247LC Superalloy Weld Heat-Affected Zone via Visualization-Based Varestraint Test
가시화 기반 Varestraint 시험을 이용한 CM247LC 초내열합금 용접 열영향부의 액화균열 민감도 평가 및 제어
Ye-Seon Jeong, Kyeong-Min Kim, Hyungsoo Lee, Seong-Moon Seo, Eun-Joon Chun
정예선, 김경민, 이형수, 서성문, 천은준
Korean J. Met. Mater. 2021;59(7):445-458.   Published online 2021 Jun 11
DOI: https://doi.org/10.3365/KJMM.2021.59.7.445

Abstract
The metallurgical aspects of weld cracking in Ni-based superalloys remain relatively unexplored in existing research. The present study performed comprehensive metallurgical and manufactural investigations into the weldability of an Ni-based superalloy, CM247LC, from the viewpoint of the liquation cracking behavior and its susceptibility. Metallurgical solutions to suppress the liquation-cracking susceptibility..... More

                   Web of Science 2  Crossref 5
Evaluation of Liquation Cracking Behavior and Susceptibility in Heat-Affected Zone of CM247LC Superalloy Welds for Turbine Blade Application
CM247LC 초내열합금 터빈 블레이드 용접 열영향부의 액화균열 발생 거동 및 민감도 평가
Ye-Seon Jeong, Kyeong-Min Kim, Uijong Lee, Hyungsoo Lee, Seong-Moon Seo, Eun-Joon Chun
정예선, 김경민, 이의종, 이형수, 서성문, 천은준
Korean J. Met. Mater. 2020;58(12):875-886.   Published online 2020 Dec 4
DOI: https://doi.org/10.3365/KJMM.2020.58.12.875

Abstract
In this study, the weldability of the as-cast CM247LC superalloy for turbine blade applications was metallurgically evaluated in terms of its hot cracking behavior and susceptibility. For this purpose, a real blade was manufactured using a directional solidification casting process, and gas tungsten arc welding was performed at the tip..... More

                   Web of Science 8  Crossref 10
Effect of Cladding Conditions on Solidification Cracking Behavior during Dissimilar Cladding of Inconel Alloy FM 52 and 308L Stainless Steel to Carbon Steel: Evaluation of Solidification Brittle Temperature Range by TransverseVarestraint Test
인코넬 FM52 및 308L 스테인리스강을 이용한 탄소강 이종 클래딩 및 공정변수에 따른 응고균열 발생 거동 변화: Transverse-Varestraint 시험을 이용한 응고취성 온도범위 평가
Yookyung Kim, Byungrok Moon, Namhyun Kang, Eun-Joon Chun
김유경, 문병록, 강남현, 천은준
Korean J. Met. Mater. 2020;58(6):403-412.   Published online 2020 May 14
DOI: https://doi.org/10.3365/KJMM.2020.58.6.403

Abstract
In this study, solidification cracking behavior and susceptibility in dissimilar cladding of Inconel alloy FM 52, 308L stainless steel to carbon steel, was investigated by submerged arc welding and transverse−Varestraint testing with gas tungsten arc welding. The effect of cladding conditions on cracking behavior and susceptibility was extensively evaluated, and..... More

                   Web of Science 6  Crossref 5
1 |
E-Submission
Email Alert
Author's Index
Specialties
Journal Impact Factor 1.2
The Korean Institute of Metals and Materials
SCImago Journal & Country Rank
Scopus
GoogleScholar
Similarity Check
Crossref Cited-by Linking
KOFST
COPE
Editorial Office
The Korean Institute of Metals and Materials
6th Fl., Seocho-daero 56-gil 38, Seocho-gu, Seoul 06633, Korea
TEL: +82-2-557-1071   FAX: +82-2-557-1080   E-mail: metal@kim.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Institute of Metals and Materials.                 Developed in M2PI