Mechanical Behavior of Spin-Coated Sb<sub>2</sub>S<sub>3</sub> light Absorption Thin Films
스핀 코팅법에 의한 Sb2S3 광흡수층 박막의 기계적 거동
Mao Zhang, Dayoung Yoo, Youngseon Jeon, Dongyun Lee
장마오, 유다영, 전영선, 이동윤
Korean J. Met. Mater. 2021;59(1):1-7.   Published online 2021 Jan 5
DOI: https://doi.org/10.3365/KJMM.2021.59.1.1

Abstract
To measure the mechanical properties of Sb2S3, a two-component compound semiconductor used in the light absorption layer of a solar cell, Sb2S3 thin films were formed on FTO glass using the spin coating method. The spin-coated Sb2S3 thin films were heat-treated at 200 oC in an Ar atmosphere for up..... More

                        
Measurement of Intrinsic Hardness of Deposited Chromium Thin Films by Nanoindentation Method and Influencing Factors
나노인덴테이션 방법으로 크롬 박막의 고유경도를 측정하는 방법과 영향 인자
Young-Joon Kang, Ju-Hwan Baeg, Hyun Park, Young-Rae Cho
강영준, 백주환, 박현, 조영래
Korean J. Met. Mater. 2020;58(3):207-215.   Published online 2020 Mar 5
DOI: https://doi.org/10.3365/KJMM.2020.58.3.207

Abstract
Materials with very small dimensions exhibit different physical and mechanical properties compared to their bulk counterparts. This becomes significantly important for the thin films that are widely used as components in micro-electronics and functional materials. In this study, a chromium (Cr) thin film was deposited on a silicon (Si) wafer..... More

                           Cited By 2
Characterization of Viscoelastic Behavior of Poly(dimethylsiloxane) by Nanoindentation
Jong-hyoung Kim, Jinwoo Lee, Woojoo Kim, Jongheon Kim, Seung-Kyun Kang, Dongil Kwon
Korean J. Met. Mater. 2019;57(5):289-294.   Published online 2019 May 5
DOI: https://doi.org/10.3365/KJMM.2019.57.5.289

Abstract
In this study, we characterize the viscoelastic behavior of polymers using nanoindentation. We applied the indentation representative stress approach and elastic solution to the Maxwell model and determined that there was a linear relationship between the inverses of the initial unloading stiffness and indentation unloading rate. From nanoindentation tests with..... More

                           Cited By 4
Effect of Oxi-Nitrocarburizing on the Microstructure, Nanohardness and Corrosion Properties for Low Carbon Steel
산질화처리가 저탄소강의 미세조직과 나노경도 및 부식특성에 미치는 영향
Young-Wook Cho, Jong-Ho Won, Jeong-Ho Woo, Sang-Ho Yu, Young-Rae Cho
조영욱, 원종호, 우정호, 유상호, 조영래
Korean J. Met. Mater. 2018;56(4):289-295.   Published online 2018 Apr 5
DOI: https://doi.org/10.3365/KJMM.2018.56.4.289

Abstract
Oxi-nitrocarburizing treatment was performed to improve the anti-corrosion and anti-wear properties of low carbon steels. The oxi-nitrocarburizing was carried out in 2 steps: a gas nitrocarburizing step at 560 ℃ and an oxidation step at 550 ℃ for 30 min with steamed water. The mechanical and chemical properties of the..... More

         Cited By 1
Influence of Nickel Thickness and Annealing Time on the Mechanical Properties of Intermetallic Compounds Formed between Cu-Sn Solder and Substrate
Cu-Sn계 솔더와 기판 사이의 Ni층의 두께와 열처리 시간에 따른 금속간화합물의 기계적 특성
Yiseul Kim, Jeehye Kwon, Dayoung Yoo, Sungkyu Park, Dajeong Lee, Dongyun Lee
김이슬, 권지혜, 유다영, 박성규, 이다정, 이동윤
Korean J. Met. Mater. 2017;55(3):165-172.   Published online 2017 Mar 3
DOI: https://doi.org/10.3365/KJMM.2017.55.3.165

Abstract
Intermetallic compounds (IMCs) developed on the interface between a solder alloy and its bonding pads are an important factor in the failure of electronic circuits. In this study, the mechanical behaviors of the IMCs formed in the Cu-Ni-Sn ternary alloy system are investigated. Presumably, Ni can act as a diffusion..... More

         Cited By 1
1 |
E-Submission
Email Alert
Author's Index
Specialties
Impact factor
The Korean Institute of Metals and Materials
SCImago Journal & Country Rank
Scopus
GoogleScholar
Similarity Check
Crossref Cited-by Linking
KOFST
COPE
Editorial Office
The Korean Institute of Metals and Materials
6th Fl., Seocho-daero 56-gil 38, Seocho-gu, Seoul 06633, Korea
TEL: +82-2-557-1071   FAX: +82-2-557-1080   E-mail: metal@kim.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Institute of Metals and Materials.                 Developed in M2PI